I suspected that might be the case. A few years back, I knew someone who did a workshop in an unnamed school and had their Dino Jacks lifted from the bench.

I got to the point when we were doing a lot of color doping of Hxtal to leave dyes from Conservation Materials out when we had students or visitors around. Dyes were not part of the class materials
.
They didn't work.
I had the good stuff put away. I did actually get calls from people trying to figure out how I was getting such nice color with them.

It's not like it once was.