Quote:
Originally Posted by Shawn Everette View Post
They made 4 clears, 5 if you count the cut off scraps. And I thought the two "studio" versions were compatible, one ate the hell out of your furnace, the other just had it for lunch.

96 is still coming out in some of the publication material, or is at least still on some of their distributor sites. I'm more concerned about their lack of transparency and surprise supply changes for all of their glass. I think their procurement of spectrum is going to make it even harder for the blowers, the amount of money they bank on tiles would make our appetite paltry. As you've said, no money in cullet.
Compatible and identical are different things. Assuming they are compatible in spec but not identical I wonder which side of the old the new one is.