I'm going to guess on the stiff side since they claim they've done away with the boric, and haven't said what else they're using for a flux.

I never tried the original "studio" nuggets, only the "new formula", which was mediocre on the blowing side, but worked fine with their sheet glass. The cut off supersaks were a mess of hot garbage. Dirty, stiff, corrosive, didn't want to fine, short pot life, and yellow. Really yellow. Though you could collect some interesting stalactites from opening of the furnace.
****
So, what about it did you not like?
__________________
Where are we going and why am I in this basket?