on the other hand copper carb is chock full of oxygen which doesn't particularly bother me since I tend to overwhelm it with stannous oxide. Do not think that stannous and stanic sound so much alike that they should be interchangeable. They aren't. Your white tin won't work.

I think starting with red is not the best plan since it's a very toucy color to achieve. Better maybe to start with the simpler stuff and just become familiar with the processof mixing and melting first..

..and there isn't that much potassium in tartar sauce. I think the formula is KNa2C4O6.4H2O so it's sort of a mixed bag I think I remember that since I was sending some to Mark Peiser two days ago and I actually bothered to read the bottle.