I suspect copper could approach or surpass the selenium reds in the right overlay situation. All by itself, no. Although I wonder what might be done based on the recipe in the archives here that combined silver with the copper ruby. The silver yellow might be a nice color tone addition to copper red.

Charles, Barb, Rich and I saw a copper ruby vase in the Tiffany show that we all declared our favorite piece without input from each other. Wet dream red like we've never seen before.

That's good to know you're still game to sell some black tin. If anyone else wants some and can't swing the $100 I'll go in with you. I still have plenty but I'll offer that in case it's needed.