I used to have one Jeff Lindsay made but I sold it when I left Santa Fe. Josh Simpson has one that runs the cane in at a 45 degree angle so that gravity feeds the machine. It just has a simple cam that raises and lowers the carbide bit. It does a lot of murrini but I never saw it do 3/4 inch which had better be annealed well and have the expansions on the money or you'll get frit.