donald Carlson did this in Oregon quite a few years back. You might try contacting him. Sinotte was never shy about the price he asked for that oval crucible. Both LaClede and Engineered ceramics did make the pot but it was considered proprietary since it wasn't round. You might see if they both still feel that way.