well, how well a murrini cuts on a saw is a pretty fair indicator of the compatibility of the contents of the murrini. The same goes if you try to nip them off. Usually, once a murrini or cane gets bigger than 1/2 inch, it has to be annealed before rendering it. So, try making the same size piece in clear only and see how it behaves , both annealed and unannealed.