Spectrum is not worth it to me to fight about. They claimed they wanted to service the glass community. That they did offering up products that did not even fit each other and frequently failed to fit substantial volumes of commercial color. Only after making Spectrum 2.0, a Spruce Pine clone short a bit of lithium and obtained under questionable circumstances did they make anything really workable. That was followed by inevitable furnace failures in which many many stones showed up in the bags and the company tried to dismiss that problem.

Not a group that I will miss.