Originally Posted by Ted Trower View Post
Just finished the test Pete suggested. Kiln did come to the desired 850 with the extension wire removed from the circuit.
****
So if I understand you, the kiln will perform as expected IF you remove the extension wire. I would suggest using a completely different wire. The one you are using may actually have a defect hidden under the insulation.