Quote:
Originally Posted by Pete VanderLaan View Post
****
So if I understand you, the kiln will perform as expected IF you remove the extension wire. I would suggest using a completely different wire. The one you are using may actually have a defect hidden under the insulation.
Thank you. Will give that a try.