I was working with the color again today and it started to get a little muddy. Remembered what Pete posted once about hitting it with acetylene to "wake it up" and it seemed to help.
I'll try the copper addition and will get back to the cobalt as well.
I found that it could also be left on the surface and even did a stannous treatment that looked really nice.
|