Volf is easy compared to Weyl. I thought the Helmer to be around forty bucks. It is only recipes, no 'splainin' nuttin". That's true of Lyngaard as well. If indeed I ever finish writing mine, which has been on a back shelf about eight years now, the intent is to try to guide the user through what's happening, how to get furnace conditions right so they will happen, expected temperature ranges for different kinds of melts, how to adjust expansion, blah blah blah.

That book has never existed.