I get it cold enough that I can handle everything. When it's first coming apart I use Kevlar mitts.Then I go away for a while. Patience is a virtue. If it needs air chiseling, I want it down around 140F.

Charlie and I are sitting down this weekend bashing on design issues. It's way too early to think about kits. Right now we're working on a prototype for the 24 inch pot that has the elements going down below pot line by about five inches. I want to see the lower half of the furnace getting some heat.