I read the super Kanthal handbook and it indicates that the elements are not prone to thermal shock. It is certainly true that you can hot change an element. I don't try to tear things down until I can actually touch the materials without wanting to drop them. I think that would be a good goal when handling the elements or passage bricks. Don't drop them!

So, while there are a myriad of ways to break elements, thermal shocking would not be one of them. Try putting them in a trebuchet and see what that gets you. Shoot for the Nebraska Line.