Quote:
Originally Posted by Franklin Sankar View Post
I am sure Jordan is better than any of the lic people, what prevents him from doing a repair according to code.
Franklin
****
I have no doubt you are correct. Jordan does not have an electricians license nor does he have liability insurance when the client is not a happy camper.

I have not tried my fix on staying above 1200F to any extent. So, I don't know. You could always try it. Make the twist good and tight. Clean the joint if you touch it. An SCR would really help.