So here we go again compatible issues, just cant understand, Ive been blowing glass for 29 years or so, and Iíve had one piece breaking unexpectedly
Ive done thousanda of cut off and polished pieces, Ive tried to estimate how many I have made, maybe 30000 Ive used Kugler Zimmarman Richenbach Only problem with opaque reds yellow and opaline white on small pieces
What is wrong in the US?
Nobody even think about it here, its a non issue, I canít understand what the problem is