As a generalization. Gaffer will give the best assurances on fit with a 96. There are issues with some phosphates, particularly containing copper which as an additive to glass has some rather unpredictable results. I make my own when I need it. The Bross formula is really a great place to start. It's not toxic and will teach your classes some pretty useful information, plus you get a good opal.