Thread: Drinkware/color
View Single Post
  #6  
Old 05-09-2020, 10:07 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,115
Pete VanderLaan is on a distinguished road
No lead poisoning, nor will there be. The notion of lead leech can occur with decanters made with lead which are almost non existent now. If the liquor stayed in the decanter long enough, it could show contaminants. Not true of glasses that get poured and drunk quickly. I don't think it's a serious issue if you are making stuff for small sales.

What you will have trouble with are businesses that will require "Proof" to release liability. Best to not deal with them. That mindset is already antithetical to the notion of handmade things.
__________________
Where are we going and why am I in this basket?
Reply With Quote