Originally Posted by Lawrence Duckworth View Post
😂 ...on average I would say my pumpkins weighed about 3 lbeez...paperweights are pretty thick too.

My point was mostly directed to the cost of ifb being a non issue.....🤔 does that make any cents
***

make a few witness weights Lawrence. Just straight clear and make them exactly the way you would do your regular production. Then Check them in a polarimeter. If it's mostly grey, you're fine. If it has a presentation of color(s) or big "X" s you're stressed.