secret ingredient!

Mark spilled the beans! He says the secret ingredient is NaC03!!

I have here a proposed application method.


Take ten lbs of mason jars, mined from the mason mt reserve outside the Anchor Hocking elysian fields of New Jersey . Clean carefully.

TO MAKE A 90 coe, ADD 90 TEASPOONS OF MAGIC POWDER. FOR A 96 coe ADD 96 TEASPOONS OF MAGIC POWDER. FOR A 104, ADD 104 TEASPOONS. On and on. The harder part comes for making a 33 coe. We'll get back to you but, it involves (wink) boron.

Stir and mix well and add to your furnace container, Wait forever.