Chords come using musical instruments. Cords are inhomogeneities in glass.

It would not surprise me to see cording when you are switching from one glass to another. Cleaning your pot well, then running one wash load, throwing that away and then just melting should yield a reasonable glass. People don't like throwing away glass at $1.50 lb.

It's a cost of doing business.