I have an optical thermometer, it matches a glowing wire to whatever you aim it at, so I dont have to be questioning the temperature. But ok Ill agree to a small extent that what youre making could demand a small change. The main point I was making was that 2150 works fine to melt cullet overnight, at least my own Glasma. It seems odd that you would have to ramp up to a normal working temperature to melt cullet