Quote:
Originally Posted by Pete VanderLaan View Post
Brian:
How is it affecting your pot? Do I recall correctly that you have a moly as well?
Yes to moly.

Crucible isn’t too bad right now. Some pitting but the crucible only has 4 months on it. I expect this to accelerate as the crucible gets to middle age.