Could loading too slow be a problem? I know the first cristalica I got was the bird turd shape not the patties. If I loaded too slow with the bird turd shape I got lots of small bubbles. If I loaded faster the hole in the shape gave larger bubbles deeper but these took the small bubbles with them when they came up and gave me great looking glass. With the patty shapes the glass had more small bubbles Just a thought.