I just don't recqll it but lithium is quite capable of causing cords all by itself. The fact that David could torch out a cord has a lithium presence to me. If you can find the source claiming the presence of lithium, I'd appreciate it.

Way back around 1975, Henry Summa and I made a lithium glass that was incredibly thermal shock resistant. You could just keep it out of the glory hole forever. Then, on the third day it was the most cordy glass I''ve ever seen. I'll never forget it.