I can’t believe I bought a controller for my furnace and can’t find any programming to ramp it up.
What a waste. I can’t believe they sell a controler you can’t ramp up.
Franklin
***
Well indeed they do. Ramp and soak has gotten more, not less expensive over time. Read the fine print, and then, read it again. I have multiple useless controllers here from Dwyer that do set point and no more. They have their uses but rarely do things a person wanting to cool products slowly would want. In LOVE, the 16 A is miles from the 16 B.