Quote:
Originally Posted by Sky Campbell View Post
Bomex is one of the largest producers of boro in China. The Chinese white is from when Paul Trautman “North Star glass” took the tag line and had it made in China. I apologize if that info is sensitive but so many years later I do believe it’s common knowledge.
Yes but its not about the formula. Pauls whites are great. For whatever reason the China white is inconsistent to the point of being unusable batch to batch. If you like it Ill sell you my 4 pounds cheap cheap.
Reply With Quote