I also spent a bit of the day reviewing the differences between Cr3 and Cr6 differences as to toxicity and color. It was a good part of the State of Oregon vs Bullseye glass. That Cr6 is Erin Brockovich land. You ain't gonna get that lime green with a Cr3 and all of that depends on furnace atmosphere.
Scholes has an excellent quote from Morey on the glassy state. Just really good explaining why things go south... and why shouldn't they? "It's only glass. "( Steve Weinberg)