I used to have great success with using dental investment plaster to form a 1 to 2 inch skin around my wax and then made a 50/50 plaster silica mix that I reinforced with stainless pins that are sold as a refractory reinforcement. In my opinion the steam release of a wet mold will give you flashing problems more than what material you use so take that into consideration