before you get too far committed, test the bomma cullet out first.

I took a few handfuls of the bomma cullet and threw them in a simple fiber board square mold to see how that would go. Mine came out a devitrified, cordy looking mess.

I suspect that the glass needs furnace temps for a full melt first.

Admittedly, mine was a one off attempt but I can get good clear castings from cristallica that has been through the furnace already.