Works really well for us. My learnings on it are. Don't count on a squeeze, just doesn't squeeze much. Don't batch in any depth, deep batching equals seeds, shallow batching equals clear. Don't batch once a week, see the depth thing. Batch when you need it. If you run way down, work your way back up over a couple of days. We keep it at 2150 and if we have a little more than usual to batch run it up to 2175. From the experiences others are having we never take it above 2175 (haven't needed to) as some folks have seen some cords when going really hot. It is really nice stuff, just behaves different than the Sys 96 studio nuggets and Cristalica.