It's been great for us so far too. I actually prefer it being a little shorter than spb for my production stuff, don't have to wait between steps for it to cool. Still longer than spectrum/oceanside or cristalica. They've kept the price drop after that bad batch, so it's kind of hard to beat at the moment.

Technically we are cooking and using it "hotter" at 2175 in our new furnace, but that's because of the thrmo being mounted on the side vs the top. We're not getting the same 'heat" we used to, the color is just not right at the old 2080.