My condolences Steve.

Schott crystal is really the go to clear, but it can be hard to come by anymore. Gaffer has some really nice colored billets, but sometimes has production availability issues. Bullseye's probably the cheapest "casting" glass, but will the more difficult to work with. I don't know anyone that's ever used Reichenbach, don't care for the pallet and OCR is still down so you can't even browse. I can't really recommend any "furnace" glass, has the wrong properties at the wrong temperatures.