I've had good results with Bullseye and Gaffer, and Spectrum when they were making it. I prefer Gaffer, it comes out of the mold cleaner and fires at a lower temp. Even after considering the different densities Gaffer is cheaper. It does look like Gaffer is out of billets though.
|