Please allow me to tell a story related to your post.
I just got a piece of grey boad and was told that it is silicaboard and the btu/ft hr deg F is .11 at 1832 F. That sounds too good to be true. Is that posible. Any guesses what it is?
They are building a new plant and I get to wallow in the garbage, found some scraps no specs and no one will say what it is.
Its a pig delight now to find some ears to show Pete.

Is there such a thing as silica board that can go up to 2300F?

Franklin
Reply With Quote