I have a real problem with putting material under something that weighs 2000lbs that is soft like Insblock or fiber. I think it is just asking for a shift off of level. I can see building it with an outer foundation load bearing wall and filling in the central area with better insulating materials, but not ever using them in a load bearing part..

Floors of furnaces are the most neglected part of them. It is a huge face for heat loss and it is never in our consciousness since we can't see it or feel it. It's there. It needs at least eight inches of insulation.