I'm looking at converting an old element furnace I have into a multi-color pot test furnace. I want to try some of these things on a smaller scale before going into my 17 lb pots. The C5.5 here looks good.
http://www.sundanceglass.com/cruciblesr.php

I actually bought one when determining what I would use in my current setup but went with two C7.1s instead. These little guys are well made and really last (and cheap!).

It would require a lot of testing no doubt. I'm more interested in trying out many different colors in opal phosphate. BUT...a nice cobalt luster would be pretty sweet. Good winter project.