View Single Post
  #4  
Old 11-06-2019, 06:07 PM
Paul Stout Paul Stout is offline
Registered User
 
Join Date: Aug 2015
Location: Tucson AZ
Posts: 18
Paul Stout is on a distinguished road
Thanks Kenny, Ill make a note. Theres a bit of zinc oxide in the East Bays batch and I had wondered if that would adversely affect the color but I guess not, thanks for the tip
Reply With Quote