View Single Post
  #5  
Old 09-18-2020, 06:12 AM
Pete VanderLaan's Avatar
Pete VanderLaan Pete VanderLaan is offline
The Old Gaffer
 
Join Date: Apr 2002
Location: Chocorua New Hampshire
Posts: 22,199
Pete VanderLaan is on a distinguished road
I am encouraging you to try to get away from the dichromate. It does produce hexavalent chromium which is well established as a carcinogen. Iron chromite would help with making the bottle green without those same issues. The great difficulty with chrome is its refractory nature and inability to be taken into solution. I have not been out to the studio to pursue recipes in the library but John Croucher and I were discussing this very issue a few months ago.
It would help to place any chromium compound you use in some lithium carbonate prior to the overall mix giving it a nice bath in some pretty aggressive stuff. I do that when making my dense black. These days, I use a juicer I got at a flea market. I got lots of them actually. They never last all that long.

I don't see why manganese would be helpful at all.
__________________
Where are we going and why am I in this basket?
Reply With Quote