I just wish they would make premium nuggets compatible. I make a line a production dicro implosion paper weights and after two days of losing 60 to 70 weights I gave up. The premium isn't even compatible with the system 96. I know because the dicro I use is all coated on system 96.

I have never had a problem in blown ware but then again I don't make thick chunky stuff. I would still like them to revist the comparability issues.