To my eye looking at your images, I'd say it is not a compatibility issue. I say that based on the fractures not appearing to have anything to do with the patterning or layering. You mention an old studio and not having problems. I'm guessing that this piece got put away a little cool and the stress from putting it away was not removed when annealing. I think the culprit is in your process somewhere. What do your polarized lenses show? My 2 cents worth.