From what the hoard says, and anecdotal personal experience, the red "Studio 96" is 94, and so is the sheet.

If the Oceanside nuggets are following the flat compatibility trend, then they too should be a 94. D&L says "96 coe" while also saying "tested compatible to strict System 96 standards'. Oceanside itself is rather mum on the subject.

First load of Bomma goes in today, so the point is moot for me now.