I've tried venting with a 1" inside diameter vent out the top. Using the nuggets, the vent was destroyed quickly. Buildup around the ceramic tube and then eventually total failure, meaning the tube dissolved.
In the larger furnaces, I can't imagine anything working to vent the nugget fumes. It's like trying to find a container for the world's strongest acid.
Now with SP, and no vent, I've really not seen a need for venting, at least for my 250 lb. and 80 lb. furnaces.