Thanks for giving me some feedback Pete. I thought my process for testing the rings should be ok but last night's result really surprised me.

I'll keep your points in mind when I test again this weekend. I do have Glassnotes and will look over the relevant sections.

Thread tests looked fine which also puzzled me, but I noted that it's not the most definitive test out there.