I have to say that I tried a few different ways. I gathered a little clear then a little brossphate side by side. One time I pulled the thread right out of the pot, but also tried it after cooling and heating a couple times. The threads were never reheated just the side by side gobs on a punty. No matter what they just stayed straight as a string.

Ring test is much more telling.