Weyl suggests that chalcedonia is actually easier in a phosphate base. If you don't have weyl ( Coloured Glasses 1951, 1954 ) , get it. It's a very though read, particularly compared to Volf but in actuality, Both authors are quite dismissive of silver bearing glasses except in silver staining. It is a real fugitive and despite rigorous control it's going to give you a good deal of heartache for no discernable reasons.