Quote:
Originally Posted by Greg Vriethoff View Post

Not the number I ever saw numerous times under a polariscope.
Do they have a polariscope that gives a number reading or are you referring to a dilatometer? If itís a dilatometer then itís very possible you used a different tempature range to test in which in return will give you different numbers.