If I had it to do over again I don’t know that I would use an expensive controller, I think I paid 15-1600 bucks a piece for these and all I do is turn them on and off....I don’t run a program anymore, they cool so slow I don’t need to.
They hold the heat and are still around 250/350 in the morning after cooling through the night. I’ve done it this way with pumpkins and paperweights since 2014 without any problems

......would the cost of the extra fire brick to do the walls and ceiling be offset by eliminating the cost of an expensive controller and the electricity to run the annealer every night all night?