Thread: Studio fire
View Single Post
  #6  
Old 07-15-2020, 03:10 PM
Steven O'Day Steven O'Day is online now
Registered User
 
Join Date: Jun 2002
Location: portland oregon
Posts: 334
Steven O'Day is on a distinguished road
I just replaced a rubber hose to a 20# propane tank. It was about 4 years old but had been outside. It seemed to be ok until it was flexed and then you could hear the gas escaping along multiple cracks.